Precision of nanoindentation protocols for measurement of viscoelasticity in cortical and trabecular bone.

Added 4299 days ago (16.08.2010)
Authors: Isaksson H, Nagao S, Małkiewicz M, Julkunen P, Nowak R, Jurvelin JS