Metals, Vol. 12, Pages 76: Stress Corrosion Analysis and Direct Cell Viability of Biodegradable Zn-Fe-Ca Alloy in In-Vitro Conditions

Added 223 days ago (03.01.2022)
Authors: Orit Avior; Noa Ben Ghedalia-Peled; Tomer Ron; Jeremy Goldman; Razi Vago; Eli Aghion